All-State Overlay 5759HW

Excellent toughness metal-cored hard overlay with good abrasion resistance and heat resistance to up to 1100°F (599°C) and still maintains a good cutting edge. Use with CO2, but best results are obtained with Argon/CO2 mixtures. Deposit hardness 57-59 RC.