This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next
ESAB

All-State Overlay 5560

All-State Overlay 5560

High carbon, high chromium, metal-cored hardfacing alloy produces wear resistant chromium carbides in a tough alloy matrix designed for high abrasion or abrasion combined with moderate impact. Use gas shielded (Argon/CO2 75/25 or Argon/Oxygen 98/2) Deposits are slag free. Use deposit thickness of 2 to 3 layers. Deposits cannot be flame cut and will check-crack to relieve stresses. Deposit hardness is 55-60 RC.

Where To Buy


x

Download the fact sheet for more information

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Overlay 5560
A/S OVERLAY 5560 1/16X25#SPL 69870468 Buy Local
A/S OVERLAY 5560 045X25#SPL 69870467 Buy Local
x
×

Find the Closest Distributor


x