All-State S-300 Black

ESAB
All-State S-300 Black

Black paste brazing flux for stainless steels, copper alloys, and steels. Performs to AWS A5.31, Type FB3-A, AMS 3410F, Mil-F-4483, and Fed OF499D. Active at 1200°F & protects to 1600°F.