This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice
All-State BRAZALOY 53'

Previous Next
ESAB

All-State BRAZALOY 53

All-State BRAZALOY 53

White powder flux for removing oxides of aluminum and zinc based alloys. Active to 700°F. Performs to AWS A5.31, Type FB1-A

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 28 ksi 371 °C

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 28 ksi 371 °C