Light blue powder flux for sheet and extruded aluminum. Removes oxides at just below the melting point of aluminun. Performs to AWS A5.31, Type FB1-A and AMS 3412D Active from 1050°F to 1250°F.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1075 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1075 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State BRAZALOY 31
A/S BRAZALOY NO 31 FLUX 8 OZ X 69080209 Buy Local
A/S BRAZALOY NO 31 FLUX 4 OZ X 69080208 Buy Local
A/S BRAZALOY NO 31 FLUX 14 OZ 69080210 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..