OK 67.45

OK 67.45

Austenitic stainless-steel electrode producing a weld metal with less than 5% ferrite. The tough weld metal has excellent crack resistance, even when welding steels with very poor weldability. Suitable for joining 12-14% manganese steel to itself or other steels. Also suitable for buffer layers before hardfacing.

Where To Buy


Specifications


Typical Tensile Properties

ISO As welded
Elongation Tensile Strength Yield Strength
35 % 88 ksi 68 ksi
AWS As welded
Elongation Tensile Strength Yield Strength
- - -

Typical Charpy V-Notch Properties

ISO As welded
Impact Value Testing Temperature
63 ft-lb 68 °F
37 ft-lb -76 °F

Typical Weld Metal Analysis %

MnMoCuCSiNiCr
6 %< 0.5 %< 0.5 %0.11 %0.50 %8.50 %18.50 %

Approvals: ABS Stainless; CE EN 13479; Sepros UNA 272580; VdTÜV 01580
Classifications: EN 1600; E 18 8 Mn B 4 2; SFA/AWS A5.4; (E307-15)

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: IMPERIAL_Stainless austenitic CrNiMn
Coating Type: Lime Basic
Ferrite Content: FN <5
Welding Current: DC+
x

Typical Tensile Properties

ISO As welded
Elongation Tensile Strength Yield Strength
35 % 88 ksi 68 ksi
AWS As welded
Elongation Tensile Strength Yield Strength
- - -

Typical Charpy V-Notch Properties

ISO As welded
Impact Value Testing Temperature
63 ft-lb 68 °F
37 ft-lb -76 °F

Typical Weld Metal Analysis %

MnMoCuCSiNiCr
6 %< 0.5 %< 0.5 %0.11 %0.50 %8.50 %18.50 %

Approvals: ABS Stainless; CE EN 13479; Sepros UNA 272580; VdTÜV 01580
Classifications: EN 1600; E 18 8 Mn B 4 2; SFA/AWS A5.4; (E307-15)

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: IMPERIAL_Stainless austenitic CrNiMn
Coating Type: Lime Basic
Ferrite Content: FN <5
Welding Current: DC+
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK 67.45
OK 67.45 2.5x300mm 1/4 VP 67452520L0 Buy Local
OK 67.45 3.2x350mm 1/2 VP 67453230T0 Buy Local
OK 67.45 4.0x350mm 1/2 VP 67454030G0 Buy Local
OK 67.45 5.0x350mm 1/2 VP 67455030G0 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..