All-State Silicon Bronze

A bare filler metal for fabricating and joining silicon bronze, copper alloys, some iron-base metals, and thin gauge galvanized steel. Deposits are high strength, ductile, and crack resistant. Use with 100% Argon or 25%/75% Argon/Helium shielding gas.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 53-55 % up to 58 ksi 25 ksi

x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 53-55 % up to 58 ksi 25 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Silicon Bronze
A/S SIL BRZ 045X25#SPL 69040232 Buy Local
A/S SIL BRZ 045X36X5#X30# 69030214 Buy Local
A/S SIL BRZ 1/16X36X5X30 69700090 Buy Local
A/S SIL BRZ 1/16X36X50 69030210 Buy Local
A/S SIL BRZ 3/32X36X5X30 69700091 Buy Local
A/S SIL BRZ 1/8X36X5X30 69700092 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..