All-State Silflo-5

All-State Silflo-5

A self-fluxing alloy for copper to copper joining. Use where close fit-up cannot be maintained. Use All-State S-200 flux when joining brass or bronze metals. Additional sizes available upon request. Tip of rod colored light blue.

Where To Buy


Specifications


Typical Tensile Properties

Brazing Temperature Copper Liquidus Temperature Phosphorous Silver Solidus Temperature
1300 - 1500 °F Balance % 1485 °F 6 % 5 % 1190 °F

x

Typical Tensile Properties

Brazing Temperature Copper Liquidus Temperature Phosphorous Silver Solidus Temperature
1300 - 1500 °F Balance % 1485 °F 6 % 5 % 1190 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Silflo-5
A/S SFLO-5 050X1/8X18X1# TB 69060062 Buy Local
A/S SFLO-5 1/8SQX36X10X60 69060044 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..