All-State Silflo 0

A self-fluxing brazing alloy for copper to copper joining. For tight fitting (.001" to .002") areas. Use All-State S-200 flux when joining brass or bronze metals. Tip of rod colored grey.

Where To Buy


Specifications


Typical Tensile Properties

Brazing Temperature Copper Liquidus Temperature Phosphorous Solidus Temperature
1350 - 1550 °F Balance % 1460 °F 7 % 1310 °F

x

Typical Tensile Properties

Brazing Temperature Copper Liquidus Temperature Phosphorous Solidus Temperature
1350 - 1550 °F Balance % 1460 °F 7 % 1310 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Silflo 0
A/S SILFO 0 050X1/8X18X1# 69050055 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..