All-State Low Fuming Bronze Bare

A bare torch rod for fabricating or repairing steels, cast iron, copper base metals, galvanized and malleable irons or any combination of these metals. Use All-State Brazaloy No. 1, No. 5, Brazo flux or All-State Jet Flux when using bare rod.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 60 ksi 1600 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 60 ksi 1600 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Low Fuming Bronze Bare
A/S LFB BARE 5/32X36X50 69060003 Buy Local
A/S LFB BARE 3/16X36X50 69060004 Buy Local
A/S LFB BARE 3/32X36X50 69060001 Buy Local
A/S LFB BARE 1/8X36X1# TUBE 69160510 Buy Local
A/S LFB BARE 1/8X36X50 69060002 Buy Local
A/S LFB BARE 1/4X36X50 69060005 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..