All-State Deoxidized Copper

All-State Deoxidized Copper

A bare filler rod that produces high purity deposits for fabricating deoxidized copper. Also used to join copper to steel or overlay them. Provides high electrical conductivity and excellent corrosion resistance. Use with 100% Argon or 25%/75% Argon/Helium shielding gas mixture.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Hardness (HRC) Tensile Strength
As Welded 40-50 % 25-40 HRC 35 ksi

x

Typical Tensile Properties

Condition Elongation Hardness (HRC) Tensile Strength
As Welded 40-50 % 25-40 HRC 35 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Deoxidized Copper
A/S DEOX CU 1/16X36X5X30 69700080 Buy Local
A/S DEOX CU 1/8X36X5X30 69700082 Buy Local
A/S DEOX CU 3/32X36X5X30 69700081 Buy Local
x
×

Find the Closest Distributor


x

Find the Closest Distributor

x

x

Loading..