ESAB
All-State 41FC

  • A premium general purpose, flux coated brazing rod for joining or overlay of steel, cast iron, brass,bronze, galvanized and malleable irons or any combination of these metals.
  • Good Color Match to Brass and Bronze
  • Excellent Machinability

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 60 ksi 1400-1650 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 60 ksi 1400-1650 °F

x