All-State 24 DC

All-State 24 DC

A DC reverse phosphor bronze electrode for welding bronze, brass, copper, cast iron, steel, and dissimilar metals. Smooth, high strength deposits can be made in all positions.

BUY NOW


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42-50 % up to 65 ksi 37 ksi

x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 42-50 % up to 65 ksi 37 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 24 DC
A/S 24DC 1/8X14X5X40 69210241 FIND A DISTRIBUTOR
A/S 24DC 3/32X14X5X40# 69201408 FIND A DISTRIBUTOR
A/S 24DC 5/32X14X5X40 69210242 FIND A DISTRIBUTOR