This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next
ESAB

All-State 24 AC DC

All-State 24 AC DC

An AC/DC all-position electrode that produces sound, porosity free deposits on bronze, brass, copper, cast iron and steel. Use as an overlay on cast iron or steel and to join dissimilar metals.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded Min. 40 % 65 ksi 37 ksi

x

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded Min. 40 % 65 ksi 37 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 24 AC DC
A/S 24AC 1/8X14X5X40# 69211009 Buy Local
A/S 24AC 5/32X14X5X40# 69211010 Buy Local