OK NiFe-CI-A'

ESAB

OK NiFe-CI-A


A nickel-iron cored electrode for joining normal grades of cast iron, such as grey-, ductile- and malleable irons. It is also suitable for rectification and repair of these grades and for joining them to steel. Deposition is done on cold or slightly preheated cast iron. The electrode produces a weld metal stronger and more resistant to solidification cracking than that of the pure nickel electrode type. It is specially suited for high duty welds in ductile irons and for welding grey irons with increased contents of sulphur and phosphorous. Typical applications include repair of pump bodies, heavy machine sections, gear teeth, flanges and pulleys.

BUY NOW


Specifications


Typical Tensile Properties

As welded
Tensile Strength
54 ksi

Typical Weld Metal Analysis

weld metal analysis
MnCSiNiAlFe
0.8 %1.5 %0.7 %51 %1.4 %46 %

Classifications: SFA/AWS A5.15; ENiFe-CI-A; EN ISO 1071; E C NiFe-CI-A 1

Alloy Type: Ni-Fe alloy
Coating Type: Basic Special high graphite
Welding Current: AC, DC+-
x

Typical Tensile Properties

As welded
Tensile Strength
54 ksi

Typical Weld Metal Analysis

weld metal analysis
MnCSiNiAlFe
0.8 %1.5 %0.7 %51 %1.4 %46 %

Classifications: SFA/AWS A5.15; ENiFe-CI-A; EN ISO 1071; E C NiFe-CI-A 1

Alloy Type: Ni-Fe alloy
Coating Type: Basic Special high graphite
Welding Current: AC, DC+-
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK NiFe-CI-A
OK NIFE-CI-A 3/32X12 6VP 9LBCT 92582520L0 FIND A DISTRIBUTOR
OK NIFE-CI-A 1/8X14 6VP 9LB CT 92583230L0 FIND A DISTRIBUTOR
OK NIFE-CI-A 5/32X14 6VP 4LBVP 92584030G0 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..