OK NiCu 1 is a nickel-copper electrode of the monel-alloy type for welding all types of cast iron with or without low preheat. The weld metal is easily machinable and produces a colour very similar to that of cast iron.

BUY NOW


Specifications


Typical Tensile Properties

ISO As welded
Elongation Tensile Strength
15 % 43.5-51 ksi

Typical Weld Metal Analysis

weld metal analysis
MnCuCSiNiFe
0.9 %32 %0.45 %<0.2 %63.5 %3 %

Classifications: EN ISO 1071; E C NiCu 1

Alloy Type: Nickel-copper alloy
Coating Type: Basic Special
x

Typical Tensile Properties

ISO As welded
Elongation Tensile Strength
15 % 43.5-51 ksi

Typical Weld Metal Analysis

weld metal analysis
MnCuCSiNiFe
0.9 %32 %0.45 %<0.2 %63.5 %3 %

Classifications: EN ISO 1071; E C NiCu 1

Alloy Type: Nickel-copper alloy
Coating Type: Basic Special
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK NiCu 1
OK NiCu 1 2.5x300mm 1/4 VP 92782520L0 FIND A DISTRIBUTOR
OK NiCu 1 3.2x350mm 1/4 VP 92783230L0 FIND A DISTRIBUTOR
OK NiCu 1 4.0x350mm 1/2 VP 92784030G0 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..