OK Ni-CI is a nickel cored electrode for joining normal grades of cast iron, such as grey-, ductile- and malleable irons. It is also suitable for rectification and repair of these grades and for joining them to steel. Deposition is done on cold or slightly preheated cast iron. Weld metal is well machinable. Typical applications are repair of cast iron parts such as cracks in engine blocks, pump housings, gear boxes, frames as well as foundry defects.

BUY NOW


Specifications


Typical Tensile Properties

As welded
Tensile Strength
43.5 ksi

Typical Weld Metal Analysis

weld metal analysis
MnCuCSiNiAlFe
0.2 %0.3 %1.0 %0.3 %93.5 %0.1 %4.5 %

Classifications: SFA/AWS A5.15; ENi-CI; EN ISO 1071; E C Ni-CI 3

Alloy Type: Ni-base alloy
Coating Type: Basic Special high graphite
Welding Current: AC, DC+-
x

Typical Tensile Properties

As welded
Tensile Strength
43.5 ksi

Typical Weld Metal Analysis

weld metal analysis
MnCuCSiNiAlFe
0.2 %0.3 %1.0 %0.3 %93.5 %0.1 %4.5 %

Classifications: SFA/AWS A5.15; ENi-CI; EN ISO 1071; E C Ni-CI 3

Alloy Type: Ni-base alloy
Coating Type: Basic Special high graphite
Welding Current: AC, DC+-
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Ni-CI
OK NI-CI 3/32X12 6VP 9LB CT 92182520L0 FIND A DISTRIBUTOR
OK NI-CI 1/8X14 6VP 10LB CT 92183230L0 FIND A DISTRIBUTOR
OK NI-CI 5/32X14 6VP 5LB VP 92184030G0 FIND A DISTRIBUTOR