All-State SUPER 4-60'

ESAB

All-State SUPER 4-60

All-State SUPER 4-60

Unique AC/DC straight or reverse electrode for heavy sections of cast iron, ductile iron and dissimilar metals. Strong, machinable,crack resistant deposits without porosity, yet spatter free. No overheating at rated amperage. Good color match.

BUY NOW


Specifications


Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 4-12 % 200-300 BHN up to 80 ksi up to 60 ksi

x

Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 4-12 % 200-300 BHN up to 80 ksi up to 60 ksi

Extra Information

Clean weld area. Vee cracks using All-State Chamfer Rod. Critical applications require preheating of 500° - 600°F( 260°- 316°C) Maintain this temperature throughout entire welding operation. Peen lightly after each weld bead. Remove all slag between passes. Use a skip welding technique.Upon completion,cover casting and allow it to cool slowly.|

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State SUPER 4-60
A/S SUPER 4-60 DSPL PK (8RODS) 69001001 FIND A DISTRIBUTOR
A/S SUPER 4-60 1/8X14X5#X40# 69010018 FIND A DISTRIBUTOR
A/S SUPER 4-60 1/8X14X10X40 69010019 FIND A DISTRIBUTOR
A/S SUPER 4-60 5/32X14X10X40 69010024 FIND A DISTRIBUTOR
A/S SUPER 4-60 1/8X14X1# 69011022 FIND A DISTRIBUTOR
A/S SUPER 4-60 3/32X12X1# 69011023 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..