Continuous flux cored DC reverse composite electrode for joining cast iron to itself or mild steel. Use with 98% Argon/2%Oxygen shielding gas.Machinable.

BUY NOW


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength
As Welded 12 % 73 ksi

x

Typical Tensile Properties

Condition Elongation Tensile Strength
As Welded 12 % 73 ksi

Extra Information

For best results,set wire amperage and adjust voltage for smoothest operation.Use 98% Argon 2% Oxygen shielding gas. Wire will also operate in the short circuiting mode or with pulse arc,and under these conditions,may be usable out-of-position.Observe the usual precautions on preheat,joint preparation,and welding technique used with other cast iron welding processes.Light peening of each bead will reduce internal stresses and minimize cracking tendencies.|

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State Corecast 8600
A/S CORE-CAST 8600 035X15# SPL 69807048 FIND A DISTRIBUTOR
A/S CORE-CAST 8600 045X15# SPL 69807049 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..