All-position AC/DC reverse nickel electrode for heavy sections of cast iron and ductile iron. For production welding requiring machinable deposits with high strength and good ductility. Good color match. Meets AWS A5.15, Class ENiFe-Cl-A

BUY NOW


Specifications


Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 4-12 % 200-300 BHN up to 80 ksi up to 60 ksi

Classifications: AWS A5.15

x

Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 4-12 % 200-300 BHN up to 80 ksi up to 60 ksi

Classifications: AWS A5.15

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 8-60
A/S 8-60 3/32X12X5 (NICKEL 55) 69020010 FIND A DISTRIBUTOR
A/S 8-60 1/8X14X5X40 69020011 FIND A DISTRIBUTOR
A/S 8-60 1/8X14X10X40 69020012 FIND A DISTRIBUTOR
A/S 8-60 5/32X14X5#X40# 69020013 FIND A DISTRIBUTOR
A/S 8-60 5/32X14X10 (NICKEL 55 69020014 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..