Premium AC/DC reverse, all-position electrode for welding thin sections of cast iron. Provides dense, machinable non-cracking, porosity free welds. Good color match. For filling defects repairing cracks, and build-up repair.

BUY NOW


Specifications


Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 2-4 % 175-225 BHN up to 50 ksi up to 40 ksi

x

Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 2-4 % 175-225 BHN up to 50 ksi up to 40 ksi