Top quality most machinable bare rod for TIG welding of thin sections of cast iron up to 3/8". Also joins cast iron to mild steel.

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength Yield Strength
As Welded up to 80 ksi up to 60 ksi

x

Typical Tensile Properties

Condition Tensile Strength Yield Strength
As Welded up to 80 ksi up to 60 ksi