All-State 4-60'

ESAB

All-State 4-60

All-State 4-60

Premium AC/DC reverse,all-position electrode for heavy sections of cast iron and ductile iron. For general maintenance welding requiring high strength, machinable deposits. Good color match. Excellent for ferrous metals high in phosphorus content.

BUY NOW


Specifications


Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 4-12 % 200-300 BHN up to 80 ksi up to 60 ksi

x

Typical Tensile Properties

Condition Elongation Hardness (BHN) Tensile Strength Yield Strength
As Welded 4-12 % 200-300 BHN up to 80 ksi up to 60 ksi

Extra Information

Preheating to 600°F(316°C) is recommended to decrease stresses and increase tensile strength and ductility. Removing all foreign material by grinding or other means and then searing the iron with a highly oxidizing torch flame will help to eliminate porosity. When welding cast iron to steels,the procedure should be the same as if two pieces of cast iron are being joined together.|

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 4-60
A/S 4-60 3/32X12X5X40VALP 69010010 FIND A DISTRIBUTOR
A/S 4-60 1/8X14X5X40 VALP 69010011 FIND A DISTRIBUTOR
A/S 4-60 1/8X14X10X40VALP 69010012 FIND A DISTRIBUTOR
A/S 4-60 5/32X14X10X40 69010014 FIND A DISTRIBUTOR