A premium DC reverse, all-position aluminum electrode with an extruded coating. For use on aluminum sheets, plates and castings of 1/8" thickness or heavier. Deposits are dense and smooth, and provide good color match to base metal. Also for build-up, cladding and reinforcing.

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength
As Welded up to 34 ksi

x

Typical Tensile Properties

Condition Tensile Strength
As Welded up to 34 ksi

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 34
A/S SMTHCTE 34 5/32X14X5# 69010054 FIND A DISTRIBUTOR
A/S SMOOTHCOTE 34 1/8X14X5X20 69010053 FIND A DISTRIBUTOR
A/S SMOOTHCOTE 34 3/32X14X5X20 69010049 FIND A DISTRIBUTOR
A/S SMOOTHCOTE 34 1/8X14X1#T 69011053 FIND A DISTRIBUTOR
A/S SMTHCTE 34 8 Rods DIS PK 69001006 FIND A DISTRIBUTOR
A/S SMTHCTE 34 3/32X14X1# 69011049 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..