All-State 31

ESAB

All-State 31

All-State 31

A special brazing alloy for joining light gauge aluminum. Used extensively in production and maintenance brazing of aluminum except 2011, 2014, 2017, 2024 and 7075 types. Alloy is very fluid and has capillary action similar to silver brazing alloys. Use with All-State 31 flux.

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1075 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1075 °F

x