Non-corrosive, non-hygroscopic flux inside a tubular rod; no separate flux required. For joining light gauge aluminum as used in furniture, truck and trailer bodies, window frames, aircraft instruments. Excellent color match but will darken if anodized. Very fluid, capillary action similar to silver brazing alloys.

BUY NOW


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1075 °F

x

Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1075 °F

x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : All-State 31 Flux Cored
A/S SUPER 31FC 1/16X18X1#T 69010040 FIND A DISTRIBUTOR
A/S SUPER 31FC 1/16X18X2OZ 69010042 FIND A DISTRIBUTOR
A/S SUPER 31FC 1/16X18X4OZ 69010045 FIND A DISTRIBUTOR
A/S SUPER 31FC 3/32X18X4OZ 69010046 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..