A ferritic, stainless, solid wire with a content of 18% Cr and stabilised with 0.5% Ti for welding similar and matching steels. The alloy is also used for cladding on unalloyed and low-alloyed steels. OK Autrod 430Ti is also widely used in the automotive industry for the welding of manifolds, catalytic converters and exhaust pipes.

BUY NOW


Typical Tensile Properties

Condition Stress Relieved Stress Relieved
Tensile Strength 600 MPa 580 MPa
Yield Strength 390 MPa 380 MPa
Elongation 24 % 28 %
Testing Time 0.5 hr 0.5 hr
Testing Temperature 780 degC 780 degC

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
80-190 A 1.1-3.1 kg/h 1.0 mm 16-24 V 1.1-3.1 m/min
180-280 A 2.6-4.5 kg/h 1.2 mm 20-28 V 2.6-4.5 m/min
230-350 A 3.0-5.2 kg/h 1.6 mm 24-28 V 3.0-5.2 m/min
0.0-0.0 kg/h 0.9 mm 0.0-0.0 m/min

Classifications

Wire Electrode EN ISO 14343-A : G Z 17 Ti
Werkstoffnummer : 1.4502

Approvals

Grade EN 13479
Society CE
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type 18 % Cr - 0.5 % Ti

Typical Weld Metal Analysis %

Wire Composition
C Cr Cu Mn Mo Ni Si Ti
0.07 % 17.6 % 0.10 % 0.5 % 0.05 % 0.3 % 0.9 % 0.400 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 430Ti
OK Autrod 430Ti 0.9mm 15kg 1681099820 FIND A DISTRIBUTOR
OK Autrod 430Ti 0.9mm 250kg 1681099320 FIND A DISTRIBUTOR
OK Autrod 430Ti 1.0mm 15kg 1681109820 FIND A DISTRIBUTOR
OK Autrod 430Ti 1.0mm 250kg 168110932U FIND A DISTRIBUTOR
OK Autrod 430Ti 1.0mm 250kg 1681109320 FIND A DISTRIBUTOR
OK Autrod 430Ti 1.2mm 15kg 1681129820 FIND A DISTRIBUTOR
OK Autrod 430Ti 1.6mm 15kg 1681169820 FIND A DISTRIBUTOR
x
x

x

Loading..