OK Autrod 430LNbTi
A ferritic stainless solid wire with low carbon content and excellent welding properties, 18 % Cr and stabilized with Nb and Ti, for welding similar and matching steels. OK Autrod 430LNbTi is developed and designed for the Automotive industry and used for production of exhaust systems. The wire should be used when there is a need for very good resistance to corrosion and thermal fatigue.
Recommended Welding Parameters
Wire Diameter | 0.035 in. |
Wire Diameter | 0.9 mm |
Deposition Data
Current | Deposition Rate | Diameter | Voltage | Wire Feed Speed |
100-260 A | 1.0 mm (.040 in.) | 18-28 V | ||
180-280 A | 2.6-4.5 kg/h (5.7-9.9 lb/h) | 1.2 mm (.045 in.) | 20-28 V | 4.9-8.5 m/min (193-335 in./min) |
Classifications
Wire Electrode |
EN ISO 14343-A : G 18 L Nb Ti Werkstoffnummer : ~1.4509 |
Approvals
Grade | EN 13479 |
Society | CE |
Approvals are based on factory location. Please contact ESAB for more information. |
Consumable Characteristics
Alloy Type | 18 % Cr – Nb and Ti stabilized |
Shielding Gas | M12, M13 (EN ISO 14175) |
Typical Weld Metal Analysis %
Typical Wire Composition % | ||||||||||||||
C | Cr | Cu | Mn | Mo | N | Nb | Ni | P | S | Si | Ti | |||
0.01 % | 18.5 % | 0.10 % | 0.5 % | 0.06 % | 0.017 % | 0.5 % | 0.2 % | 0.020 % | 0.005 % | 0.5 % | 0.30 % |