A continous ferritic stainless solid wire with low carbon content, 18 % Cr and stabilized with Nb, for welding similar and matching steels. OK Autrod 430LNb (W) is developed and designed for the automotive industry and used for production of exhaust systems. The wire should be used when there is a need for good resistance to corrosion and thermal fatigue. The OK Autrod 430LNb (W) is a new version of OK Autrod 430LNb, with restricted Nb limits.

BUY NOW


Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded26 %420 MPa275 MPa

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
50-140 A 0.8-2.7 kg/h 0.8 mm 16-22 V 0.8-2.7 m/min
80-190 A 1.1-3.1 kg/h 1.0 mm 16-24 V 1.1-3.1 m/min
180-280 A 2.6-4.5 kg/h 1.2 mm 20-28 V 2.6-4.5 m/min
0.0-0.0 kg/h 1.14 mm 0.0-0.0 m/min
0.0-0.0 kg/h 0.9 mm 0.0-0.0 m/min

Classifications

Wire Electrode Werkstoffnummer : ~1.4511
EN ISO 14343-A : G 18 L Nb

Consumable Characteristics

Alloy Type 18 % Cr - 0.5 % Nb

Typical Weld Metal Analysis %

Wire Composition
C Cr Cu Mn Mo Nb Ni Si
0.01 % 18.5 % 0.10 % 0.5 % 0.06 % 0.45 % 0.2 % 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 430LNb
OK Autrod 430LNb 0.8mm 15kg 1676089820 FIND A DISTRIBUTOR
OK Autrod 430LNb 0.8mm 200kg 1676089300 FIND A DISTRIBUTOR
OK Autrod 430LNb 0.9mm 250kg 1676099320 FIND A DISTRIBUTOR
OK Autrod 430LNb 1.0mm 100kg 1676109500 FIND A DISTRIBUTOR
OK AUTROD 430LNB 039X33#SP 1676109820 FIND A DISTRIBUTOR
OK Autrod 430LNb 1.0mm 15kg 1676109800 FIND A DISTRIBUTOR
OK AUTROD 430LNB 039X550#OMP 1676109320 FIND A DISTRIBUTOR
OK Autrod 430LNb 1.0mm 250kg 167610932U FIND A DISTRIBUTOR
OK Autrod 430LNb 1.0mm 500kg 1676109A00 FIND A DISTRIBUTOR
OK AUTROD 430LNB 047X33#SP 1676129820 FIND A DISTRIBUTOR
OK Autrod 430LNb 1.2mm 250kg 167612932U FIND A DISTRIBUTOR
OK Autrod 430LNb 1.2mm 250kg 1676129320 FIND A DISTRIBUTOR
x
x

x

Loading..