A continuous solid corrosion resisting chromium-nickel wire for joining stainless steels to non-alloy or low alloy steels as well as welding of austenitic stainless alloys of 24% Cr, 13% Ni, high C types. OK Autrod 309Si has a good general corrosion resistance. The higher silicon content improves the welding properties such as wetting. When used for joining dissimilar materials the corrosion resistance is of secondary importance.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
60 J (44 ft-lb) -110 degC (-166 degF)
80 J (59 ft-lb) -60 degC (-76 degF)
100 J (74 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded36 %620 MPa (90 ksi)440 MPa (64 ksi)

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
50-140 A 0.8-2.7 kg/h (1-6 lb/h) 0.8 mm (0.030 in.) 16-22 V 3.4-11.0 m/min (134-433 in./min)
80-190 A 1.1-3.1 kg/h (2-6 lb/h) 1.0 mm (0.040 in.) 16-24 V 2.9-8.4 m/min (114-331 in./min)
180-280 A 2.6-4.5 kg/h (5-9 lb/h) 1.2 mm (0.047 in.) 20-28 V 4.9-8.5 m/min (193-335 in./min)
230-350 A 3.0-5.2 kg/h (6-11 lb/h) 1.6 mm (1/16 in.) 24-28 V 3.2-5.5 m/min (126-217 in./min)

Classifications

Wire Electrode EN ISO 14343-A : G 22 12 H
SFA/AWS A5.9 : ER309Si
Werkstoffnummer : ~1.4829

Consumable Characteristics

Alloy Type Austenitic (with approx. 10 % ferrite) 23 % Cr - 13 % Ni - High Si

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu Mn Mo Ni P S Si Si+Fe
0.08 % 23.3 % 0.15 % 1.8 % 0.20 % 12.7 % - - 0.9 % 5 %
Typical Weld Metal Analysis %
0.06 % 24 % - 1.8 % - 13 % 0.015 % 0.015 % 0.8 % -
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 309Si
1652089820 FIND A DISTRIBUTOR
1652109820 FIND A DISTRIBUTOR
1652109320 FIND A DISTRIBUTOR
1652129820 FIND A DISTRIBUTOR
1652129320 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..