ESAB

OK Autrod 309LSi

The following items have been added to your list


x

A continous solid corrosion resistant chromium-nickel wire for welding of similar steels, wrought and cast steels of 23% Cr-12% Ni types. The alloy is also used for welding of buffer layers on CMn steels and welding of dissimilar joints. When using the wire for buffer layers and dissimilar joints it is necessary to control the dilution of the weld. OK Autrod 309LSi has a good general corrosion resistance. The higher silicon content improves the welding properties, such as wetting.

BUY NOW


Typical Charpy V-Notch Properties

as welded

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded35 %600 MPa (87 ksi)440 MPa (64 ksi)

Recommended Welding Parameters

Wire Diameter 0.045 in.
Wire Diameter 1.14 mm

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
80-240 A 1.5-6.0 kg/h (3.3-13. lb/h) 1.0 mm (0.040 in.) 15-28 V 4.0-16.0 m/min (157-630 in./min)
100-300 A 1.6-7.5 kg/h (3.5-16. lb/h) 1.2 mm (0.047 in.) 15-29 V 3.0-14.0 m/min (118-551 in./min)
65-220 A 1.1-5.4 kg/h (2.4-11. lb/h) 0.9 mm (0.035 in.) 15-28 V 3.5-18.0 m/min (138-709 in./min)
55-160 A 1.0-4.1 kg/h (2.2-9.0 lb/h) 0.8 mm (0.030 in.) 15-24 V 4.0-17.0 m/min (157-669 in./min)
230-375 A 5.2-8.6 kg/h (11.5-19. lb/h) 1.6 mm (1/16 in.) 23-31 V 5.5-9.0 m/min (217-354 in./min)

Classifications

Wire Electrode EN ISO 14343-A : G 23 12 L Si
SFA/AWS A5.9 : ER309LSi

Approvals

Approvals CE EN 13479
CWB ER309LSi
DB 43.039.16
NAKS/HAKC 1.0MM-1.2MM
VdTÜV 10020
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic (with approx. 8 % ferrite) 24 % Cr - 13 % Ni - Low C
Shielding Gas M12, M13 (EN ISO 14175)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu FN WRC-92 Mn Mo N Nb Ni P S Si
0.016 % 23.3 % 0.1 % 9 % 1.9 % 0.1 % 0.09 % - 13.7 % 0.019 % 0.004 % 0.7 %
Typical Weld Metal Analysis %
0.02 % 23 % 0.1 % 7 % 1.8 % 0.1 % 0.07 % 0.01 % 13.5 % 0.015 % 0.003 % 0.7 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 309LSi
1651099320 Find a distributor
1651089820 Find a distributor
1651084600 Find a distributor
1651099500 Find a distributor
1651099820 Find a distributor
1651094600 Find a distributor
1651109500 Find a distributor
1651109820 Find a distributor
1651109320 Find a distributor
1651104600 Find a distributor
1651113400 Find a distributor
1651119500 Find a distributor
1651119820 Find a distributor
1651119320 Find a distributor
1651129820 Find a distributor
165112982F Find a distributor
1651129320 Find a distributor
1651124600 Find a distributor
1651169820 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..