A continuous solid corrosion resisting chromium-nickel wire. OK Autrod 308L has a good general corrosion resistance.The alloy has a low carbon content which makes this alloy particularly recommended were there is a risk of intergranular corrosion. The alloy is widely used in the chemical and food processing industries as well as for pipes, tubes and boilers. For joining of stainless steels of 18% Cr - 8% Ni-type and Nb-stabilized steels of the same type if the service temperature will not exceed 350°C.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded
60 J (44 ft-lb) -196 degC (-321 degF)
90 J (66 ft-lb) -60 degC (-76 degF)
110 J (81 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

As welded As welded
Shielding Gas Tested at 350°C (662°F).
Tensile Strength 490 MPa (71 ksi) 620 MPa (90 ksi)
Yield Strength 370 MPa (54 ksi) 450 MPa (65 ksi)
Elongation 25 % 36 %

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
80-240 A 1.5-6.0 kg/h (3.3-13.2 lb/h) 1.0 mm (.040 in.) 15-28 V 4.0-16.0 m/min (157.5-630 in./min)
55-160 A 0.9-4.1 kg/h (2.0-9.0 lb/h) 0.8 mm (.030 in.) 15-24 V 4.0-17.0 m/min (157.5-669 in./min)
55-160 A 0.9-4.1 kg/h (2.0-9.0 lb/h) 0.9 mm (.035 in.) 15-24 V 4.0-17.0 m/min (157.5-669 in./min)
80-240 A 1.5-6.0 kg/h (3.3-13.2 lb/h) 1.14 mm (.045 in.) 15-28 V 4.0-16.0 m/min (157.5-630 in./min)
100-300 A 1.6-7.5 kg/h (3.5-16.5 lb/h) 1.2 mm (.045 in.) 14-28.5 V 3.0-14.0 m/min (118-551 in./min)

Classifications

Wire Electrode Werkstoffnummer : ~1.4316
EN ISO 14343-A : G 19 9 L
SFA/AWS A5.9 : ER308L

Approvals

Approvals ABS ER308/308L
CE EN 13479
NAKS/HAKC 1.0 mm
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic (with approx. 8 % ferrite) 19% Cr - 9% Ni - Low C

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Cu FN WRC-92 Mn Mo N Ni P S Si
0.02 % 19.8 % 0.15 % 9 % 1.9 % 0.20 % 0.05 % 9.8 % - - 0.4 %
Typical Weld Metal Analysis %
0.020 % 20.0 % 0.05 % - 1.6 % 0.05 % - 10.0 % 0.015 % 0.015 % 0.4 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 308L
1610129320 FIND A DISTRIBUTOR
161016982A FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..