ESAB

OK Autrod 308H

The following items have been added to your list


x

A continuous, solid, corrosion-resistant, chromium-nickel wire for welding austenitic chromium-nickel alloys of the 18% Cr-8% Ni type. OK Autrod 308H has good general corrosion resistance. The alloy has a high carbon content, making it suitable for applications used at higher temperatures. The alloy is used in chemical and petrochemical plants for the welding of pipes, cyclones and boilers.

BUY NOW


Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
50-140 A 0.8-2.7 kg/h (1-6 lb/h) 0.8 mm (0.030 in.) 16-22 V 3.4-11.0 m/min (134-433 in./min)
80-190 A 1.1-3.1 kg/h (2-6 lb/h) 1.0 mm (0.040 in.) 16-24 V 2.9-8.4 m/min (114-331 in./min)
180-280 A 2.6-4.5 kg/h (5-9 lb/h) 1.2 mm (0.047 in.) 20-28 V 4.9-8.5 m/min (193-335 in./min)

Classifications

Wire Electrode EN ISO 14343-A : G 19 9 H
SFA/AWS A5.9 : ER308H

Consumable Characteristics

Alloy Type Austenitic 19% Cr - 9% Ni - High C

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cr Mn Ni Si
0.05 % 19.8 % 1.9 % 9.2 % 0.5 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 308H
1615109820 FIND A DISTRIBUTOR
1615129820 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..