A continous solid corrosion resisting chromium-nickel-manganese wire for welding of austenitic stainless alloys of 18% Cr, 8% Ni, 7% Mn types. OK Autrod 16.95 has a general corrosion resistance similar to that of the corresponding parent metal. The higher silicon content improves the welding properties, such as wetting. The product is a modified variant of ER307, basically with a higher Mn content to make the weld metal less sensitive to hot cracking. When used for joining dissimilar materials the corrosion resistance is of secondary importance. The alloy is used in a wide range of applications across the industry such as joining of austenitic, manganese, work hardenable steels as well as armourplate and heat resistant steels.

BUY NOW


Typical Charpy V-Notch Properties

As Welded
Impact Value 96 ft-lb
Impact Value 130 J
Testing Temperature 68 °F
Testing Temperature 20 °C

Typical Tensile Properties

ConditionElongationTensile Strength Yield Strength
As Welded41 %640 MPa (93 ksi)450 MPa (65 ksi)

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
80-240 A 1.5-6.0 kg/h (3.3-13. lb/h) 1.0 mm (0.040 in.) 15-28 V 4.0-16.0 m/min (157-630 in./min)
100-300 A 1.6-7.5 kg/h (3.5-16. lb/h) 1.2 mm (0.047 in.) 15-29 V 3.0-14.0 m/min (118-551 in./min)
65-220 A 1.1-5.4 kg/h (2.4-11. lb/h) 0.9 mm (0.035 in.) 15-28 V 3.5-18.0 m/min (138-709 in./min)
55-160 A 1.0-4.1 kg/h (2.2-9.0 lb/h) 0.8 mm (0.030 in.) 15-24 V 4.0-17.0 m/min (157-669 in./min)
230-375 A 5.2-8.6 kg/h (11.5-19. lb/h) 1.6 mm (1/16 in.) 23-31 V 5.5-9.0 m/min (217-354 in./min)

Classifications

Wire Electrode EN ISO 14343-A : G 18 8 Mn
SFA/AWS A5.9 : ER307 mod
Werkstoffnummer : ~1.4370

Approvals

Approvals CE EN 13479
DB 43.039.10
NAKS/HAKC 1.2MM
VdTÜV 05420
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Austenitic (18 % Cr - 8 % Ni - 7 % Mn)
Shielding Gas M12, M13 (EN ISO 14175)

Typical Weld Metal Analysis %

Typical Weld Metal Analysis %
C Cr Cu Mn Mo Ni P S Si
0.1 % 18.5 % 0.1 % 6.5 % 0.1 % 8.5 % 0.010 % 0.020 % 1 %
Typical Wire Composition %
0.08 % 18.7 % 0.10 % 7.0 % 0.20 % 8.1 % - - 0.9 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 16.95
1695089820 Find a distributor
1695089300 Find a distributor
1695099820 Find a distributor
1695109500 Find a distributor
1695109820 Find a distributor
1695109320 Find a distributor
169510932U Find a distributor
1695109370 Find a distributor
1695109A00 Find a distributor
1695119820 Find a distributor
1695129500 Find a distributor
1695129820 Find a distributor
1695129320 Find a distributor
169512932U Find a distributor
1695129A00 Find a distributor
1695169410 Find a distributor

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..