A continuous solid corrosion resisting non-magnetic chromium-nickel-molybdenium wire for welding of stabilized and non-stabilized austenitic alloys of the same type as well as non magnetic steels. The alloy is corrosion resistant in seawater environment and has very good corrosion resistance to acids such as nitric acid. Excellent impact properties at low temperatures

BUY NOW


Typical Weld Metal Analysis %

Wire Composition
C Cr Mn Mo N Ni Si
0.01 % 19.9 % 6.9 % 3.0 % 0.18 % 16.5 % 0.4 %

Typical Charpy V-Notch Properties

Classifications

Name EN ISO 14343-A
Grade G 20 16 3 Mn L
2

Consumable Characteristics

Alloy Type Austenitic (7 % Mn - 20 % Cr - 16 % Ni - 3 % Mo)

Typical Tensile Properties

ElongationTensile Strength (imp)Yield Strength (imp)
40 %600 MPa (87 ksi)400 MPa (58 ksi)

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
80-190 A 1.1-3.1 kg/h(2.4-6.8 lb/h) 1.0 mm(.040 in.) 16-24 V 2.9-8.4 m/min(114-331 in./min)
180-280 A 2.6-4.5 kg/h(5.7-9.9 lb/h) 1.2 mm(.045 in.) 20-28 V 4.9-8.5 m/min(193-335 in./min)
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod 16.38
OK Autrod 316LMn 1.2mm 15kg 1638129820 FIND A DISTRIBUTOR