OK Autrod NiCrMo-13
A continuous solid Ni-Cr-Mo electrode for welding of high alloyed Ni-base materials, 9% Ni steel and super austenitic steels of type 20Cr-25Ni with 4-6% Mo. Can also be used for welding carbon steel to Ni base steel. The weld metal has a very good toughness and is corrosion resistant over a wide range of applications in oxidising and reducing media.
Typical Weld Metal Analysis %
Wire Composition | ||||||||||||||
Al | C | Cr | Fe | Mn | Mo | Ni | Si | |||||||
0.3 % | 0.01 % | 23.0 % | 1.0 % | 0.2 % | 16.0 % | bal % | 0.1 % |
Approvals
Society | VdTÜV |
Grade | 12662 (MV) |
Approvals are based on factory location. Please contact ESAB for more information. |
Typical Charpy V-Notch Properties
Testing Temperature | -110 degC |
Testing Temperature | -166 degF |
Impact Value (met) | 120 J |
Impact Value (imp) | 88.5 ft-lb |
Conditional Statement | As welded |