A continuous solid nickel based electrode alloyed with about 3% Ti for welding of high purity nickel (min 99.6%Ni), ordinary wrought nickel and nickel with reduced C content. The weld metal can be used in a wide range of applications were the construction is working with corrosive media.

BUY NOW


Typical Weld Metal Analysis %

Wire Composition
Al C Cu Fe Mn Ni Si Ti
0.06 % 0.01 % 0.01 % 0.04 % 0.4 % 96 % 0.5 % 3.1 %

Approvals

Society VdTÜV
Grade 12658 (MV)
Approvals are based on factory location. Please contact ESAB for more information.

Typical Charpy V-Notch Properties

Testing Temperature 20 degC
Testing Temperature 68 degF
Conditional Statement As welded

Classifications

Grade ERNi-1
Name SFA/AWS A5.14
Grade S Ni 2061 (NiTi3)
Name EN ISO 18274

Consumable Characteristics

Alloy Type Nickel (Ni + 2.5 % Ti)

Typical Tensile Properties

Deposition Data

Wire Feed Speed 6-13 m/min
Wire Feed Speed 236-512 in./min
Voltage 21-27 V
Diameter 1.0 mm
Diameter .040 in.
Deposition Rate 2.5-5.5 kg/h
Deposition Rate 5.5-12.1 lb/h
Current 100-200 A
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Autrod Ni-1
OK Autrod Ni-1 0.8mm 1kg 1992089820 FIND A DISTRIBUTOR
OK Autrod Ni-1 1.0mm 15kg 1992109820 FIND A DISTRIBUTOR
x
x

x

Loading..