Spoolarc 82'

ESAB

Spoolarc 82


Spoolarc 82 is a premium quality, general purpose MIG wire subjected to stringent quality control procedures required for certification to Military, Lloyds, and ABS specifications. Spoolarc 82 is recommended for pressure vessel and pipe fabrication, HVAC duct work, and general carbon steel structural welding.

BUY NOW


Industries

  • Automotive
  • Industrial and General Fabrication
  • Pipeline
  • Mobile Equipment

Welding Process

  • GTAW (TIG)
  • GMAW (MIG/MAG)

Specifications


Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 28 % 76 ksi 62 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 28 % 73 ksi 60 ksi
90% Ar - 10% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 85 ksi 72 ksi
75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 21 % 85 ksi 71 ksi

Typical Charpy V-Notch Properties

98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 83 ft-lb -20 °F
100% CO2
Condition Impact Value Testing Temperature
As Welded 75 ft-lb -20 °F
90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 65 ft-lb -45 °C
As Welded 84 ft-lb -40 °C
As Welded 96 ft-lb -20 °F
75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 58 ft-lb -45 °C
As Welded 60 ft-lb -40 °C
As Welded 73 ft-lb -20 °F

Typical Weld Metal Analysis %

wire composition
PMnMoCuSCVSiNiCr
0.011 %1.18 %0.01 %0.16 %0.007 %0.09 %0.004 %0.58 %0.02 %0.03 %

Approvals: ABS; AWS A5.18: ER70S-3 H4; CWB CSA W48; CAN/CSA-ISO14341,B-G 49A 2C G3 (ER49S-3); MIL-E-23765/1 MIL-70S-3
Classifications: AWS A5.18; ER70S-3 H4

Approvals are based on factory location. Please contact ESAB for more information.


x

Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 28 % 76 ksi 62 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 28 % 73 ksi 60 ksi
90% Ar - 10% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 85 ksi 72 ksi
75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 21 % 85 ksi 71 ksi

Typical Charpy V-Notch Properties

98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 83 ft-lb -20 °F
100% CO2
Condition Impact Value Testing Temperature
As Welded 75 ft-lb -20 °F
90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 65 ft-lb -45 °C
As Welded 84 ft-lb -40 °C
As Welded 96 ft-lb -20 °F
75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 58 ft-lb -45 °C
As Welded 60 ft-lb -40 °C
As Welded 73 ft-lb -20 °F

Typical Weld Metal Analysis %

wire composition
PMnMoCuSCVSiNiCr
0.011 %1.18 %0.01 %0.16 %0.007 %0.09 %0.004 %0.58 %0.02 %0.03 %

Approvals: ABS; AWS A5.18: ER70S-3 H4; CWB CSA W48; CAN/CSA-ISO14341,B-G 49A 2C G3 (ER49S-3); MIL-E-23765/1 MIL-70S-3
Classifications: AWS A5.18; ER70S-3 H4

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Spoolarc 82
82 030X44#SP 1212F04 FIND A DISTRIBUTOR
82 035X44#SP 1212F05 FIND A DISTRIBUTOR
82 045X44#SP 1212F07 FIND A DISTRIBUTOR
82 045X60#SP 1218F47 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..