Spoolarc 65 is a triple deoxidized (Aluminum, Titanium, Zirconium) welding wire designed for welding over rust and mill scale. The less fluid weld puddle of Spoolarc 65 makes it easy to control when used out of position. Spoolarc 65 is the preferred wire for all position welding of small diameter pipe. It is available in forms suitable for MIG and TIG welding.

BUY NOW


Industries

  • Pipeline
  • Power Generation
  • Ship/Barge Building
  • Military Applications

Welding Process

  • GMAW (MIG/MAG)

Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded gmaw 100% ar
47 J (35 ft-lb) -29 degC (-20 degF)
as welded gmaw 98% ar - 2% o2
61 J (45 ft-lb) -29 degC (-20 degF)

Typical Tensile Properties

Condition As Welded As Welded
Shielding Gas 98% Ar - 2% O2 100% Ar
Tensile Strength 565 MPa (82 ksi) 545 MPa (79 ksi)
Yield Strength 480 MPa (70 ksi) 460 MPa (67 ksi)
Elongation 26 % 26 %

Recommended Welding Parameters

Current Voltage Wire Diameter Wire Feed Speed
Short Arc Transfer Optimum
70 A 15 V 0.6 mm (.023 in.) 762 cm/min (300 in./min)
100 A 15 V 0.8 mm (.030 in.) 559 cm/min (220 in./min)
130 A 17 V 0.9 mm (.035 in.) 635 cm/min (250 in./min)
160 A 18 V 1.2 mm (.045 in.) 381 cm/min (150 in./min)
160 A 18 V 1.4 mm (.052 in.) 356 cm/min (140 in./min)
Short Arc Transfer
45-90 A 14-16 V 0.6 mm (.023 in.) 381-965 cm/min (150-380 in./min)
60-140 A 14-16 V 0.8 mm (.030 in.) 381-889 cm/min (150-350 in./min)
90-160 A 15-19 V 0.9 mm (.035 in.) 457-762 cm/min (180-300 in./min)
130-200 A 17-19 V 1.2 mm (.045 in.) 318-508 cm/min (125-200 in./min)
150-200 A 17-20 V 1.4 mm (.052 in.) 343-483 cm/min (135-190 in./min)
Spray Transfer Optimum
110 A 23 V 0.6 mm (.023 in.) 1143 cm/min (450 in./min)
180 A 25 V 0.8 mm (.030 in.) 1321 cm/min (520 in./min)
200 A 26 V 0.9 mm (.035 in.) 1219 cm/min (480 in./min)
300 A 27 V 1.2 mm (.045 in.) 889 cm/min (350 in./min)
325 A 28 V 1.4 mm (.052 in.) 787 cm/min (310 in./min)
340 A 27 V 1.6 mm (1/16 in.) 508 cm/min (200 in./min)
Spray Transfer
100-125 A 23-25 V 0.6 mm (.023 in.) 1016-1575 cm/min (400-620 in./min)
160-200 A 24-26 V 0.8 mm (.030 in.) 1270-1651 cm/min (500-650 in./min)
180-230 A 25-27 V 0.9 mm (.035 in.) 1016-1397 cm/min (400-550 in./min)
260-340 A 25-30 V 1.2 mm (.045 in.) 762-1270 cm/min (300-500 in./min)
275-400 A 26-33 V 1.4 mm (.052 in.) 673-991 cm/min (265-390 in./min)
290-400 A 26-36 V 1.6 mm (1/16 in.) 457-711 cm/min (180-280 in./min)

Deposition Data

Current Deposition Rate Deposition Type Diameter Voltage Wire Feed Speed
113 A 1.5 kg/h (3.3 lb/h) Short Arc Transfer 0.9 mm (.035 in.) 16 V 559 cm/min (220 in./min)
160 A 2.1 kg/h (4.6 lb/h) Short Arc Transfer 0.9 mm (.035 in.) 19 V 762 cm/min (300 in./min)
90 A 1.2 kg/h (2.7 lb/h) Short Arc Transfer 0.9 mm (.035 in.) 15 V 457 cm/min (180 in./min)
130 A 1.4 kg/h (3.1 lb/h) Short Arc Transfer 1.2 mm (.045 in.) 17 V 318 cm/min (125 in./min)
180 A 2.9 kg/h (6.3 lb/h) Spray Transfer 0.9 mm (.035 in.) 25 V 1016 cm/min (400 in./min)
197 A 3.2 kg/h (7.1 lb/h) Spray Transfer 0.9 mm (.035 in.) 26 V 1143 cm/min (450 in./min)
213 A 3.6 kg/h (7.9 lb/h) Spray Transfer 0.9 mm (.035 in.) 26 V 1270 cm/min (500 in./min)
260 A 3.6 kg/h (7.9 lb/h) Spray Transfer 1.2 mm (.045 in.) 25 V 762 cm/min (300 in./min)
280 A 4.2 kg/h (9.2 lb/h) Spray Transfer 1.2 mm (.045 in.) 26 V 889 cm/min (350 in./min)
300 A 4.8 kg/h (10.5 lb/h) Spray Transfer 1.2 mm (.045 in.) 28 V 1016 cm/min (400 in./min)
320 A 5.4 kg/h (11.8 lb/h) Spray Transfer 1.2 mm (.045 in.) 29 V 1143 cm/min (450 in./min)
230 A 4.0 kg/h (8.7 lb/h) Spray Transfer 0.9 mm (.035 in.) 27 V 1397 cm/min (550 in./min)
340 A 6.0 kg/h (13.1 lb/h) Spray Transfer 1.2 mm (.045 in.) 30 V 1270 cm/min (500 in./min)
290 A 4.1 kg/h (9.1 lb/h) Spray Transfer 1.6 mm (1/16 in.) 26 V 457 cm/min (180 in./min)
310 A 4.6 kg/h (10.1 lb/h) Spray Transfer 1.6 mm (1/16 in.) 28 V 508 cm/min (200 in./min)
340 A 5.3 kg/h (11.6 lb/h) Spray Transfer 1.6 mm (1/16 in.) 31 V 584 cm/min (230 in./min)
370 A 6.0 kg/h (13.2 lb/h) Spray Transfer 1.6 mm (1/16 in.) 34 V 660 cm/min (260 in./min)
390 A 6.4 kg/h (14.2 lb/h) Spray Transfer 1.6 mm (1/16 in.) 36 V 711 cm/min (280 in./min)
137 A 1.8 kg/h (4.0 lb/h) Short Arc Transfer 0.9 mm (.035 in.) 18 V 660 cm/min (260 in./min)
163 A 1.8 kg/h (4.0 lb/h) Short Arc Transfer 1.2 mm (.045 in.) 18 V 406 cm/min (160 in./min)
200 A 2.3 kg/h (5.0 lb/h) Short Arc Transfer 1.2 mm (.045 in.) 19 V 508 cm/min (200 in./min)

Classifications

Grade ER70S-2 H4
Name AWS A5.18

Typical Weld Metal Analysis %

Typical Wire Composition %
Al C Cr Cu Mn Mo Ni P S Si Ti V Zr
0.08 % 0.06 % 0.06 % 0.10 % 1.14 % 0.01 % 0.03 % 0.004 % 0.006 % 0.50 % 0.10 % 0.01 % 0.04 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Spoolarc 65
1042F04 FIND A DISTRIBUTOR
104EFBD FIND A DISTRIBUTOR
1042F05 FIND A DISTRIBUTOR
104UF65 FIND A DISTRIBUTOR
104EFDD FIND A DISTRIBUTOR
1042F07 FIND A DISTRIBUTOR
104UF67 FIND A DISTRIBUTOR
1042F08 FIND A DISTRIBUTOR
1044F28 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..