SPOOLARC 29S

Spoolarc 29S is a general purpose copper-coated solid wire suitable for many carbon steel welding applications using the MIG/Gas Metal Arc Welding (GMAW). Spoolarc 29S contains moderate amounts of manganese and silicon to provide sufficient deoxidation over light mill scale. Shielding gas choices for Spoolarc 29S in the GMAW mode are 100% carbon dioxide, argon/carbon dioxide mixtures, argon/oxygen mixtures, and other argon based mixed gas blends. Spoolarc 29S is used in a wide variety of applications including heavy equipment, automotive parts, railcars, agricultural equipment, and sheet metal welding.
Industries
- Mobile Equipment
- Industrial and General Fabrication
- Civil Construction
- Automotive
Welding Process
- GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)
Typical Tensile Properties
90% Ar - 10% CO2 | |||
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 22 % | 85 ksi | 72 ksi |
75% Ar - 25% CO2 | |||
Condition | Elongation | Tensile Strength | Yield Strength |
As Welded | 21 % | 85 ksi | 71 ksi |
Typical Charpy V-Notch Properties
90% Ar - 10% CO2 | ||
Condition | Impact Value | Testing Temperature |
As Welded | 65 ft-lb | -50 °F |
As Welded | 84 ft-lb | -40 °F |
As Welded | 96 ft-lb | -20 °F |
75% Ar - 25% CO2 | ||
Condition | Impact Value | Testing Temperature |
As Welded | 58 ft-lb | -50 °F |
As Welded | 60 ft-lb | -40 °F |
As Welded | 73 ft-lb | -20 °F |
Typical Weld Metal Analysis %
wire composition | |||||||||
P | Mn | Mo | Cu | C | S | V | Si | Ni | Cr |
0.015 % | 1.18 % | 0.01 % | 0.04 % | 0.09 % | 0.007 % | 0.004 % | 0.54 % | 0.04 % | 0.04 % |
Approvals: | ABS; 3SA, 3YSA; CWB; CAN/CSA-ISO14341,B-G 49A 2C G3 (ER49S-3); CWB; CSA W48 |
Classifications: | AWS A5.18; ER70S-3 |