Pipeweld 70S-6

ESAB

Pipeweld 70S-6

The following items have been added to your list


x

A copper coated solid wire especially designed for downhill circumferential GMAW on pipes in materials such as APi 5L (grade 52 up to grade 70). The main applications are pipelines, compressor stations and associated works in the oil and gas distribution industries with special requirements. To meet these requirements the electrode is a "clean" type of EN ISO 14341-A G4Si1 as regards chemical analysis.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded aws co2 (c1)
100 J (74 ft-lb) -20 degC (-4 degF)
80 J (59 ft-lb) -29 degC (-20 degF)
as welded en 80ar/20co2 (m21)
100 J (74 ft-lb) -20 degC (-4 degF)
80 J (59 ft-lb) -30 degC (-22 degF)
140 J (104 ft-lb) 20 degC (68 degF)
as welded en co2 (c1)
80 J (59 ft-lb) -20 degC (-4 degF)
120 J (89 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

Condition As Welded As Welded As Welded
Shielding Gas AWS CO2 (C1) EN 80Ar/20CO2 (M21) EN CO2 (C1)
Tensile Strength 575 MPa (83 ksi) 600 MPa (87 ksi) 575 MPa (83 ksi)
Yield Strength 470 MPa (68 ksi) 545 MPa 495 MPa
Elongation 29 % 26 % 25 %

Classifications

Wire Electrode SFA/AWS A5.18 : ER70S-6
Weld Metal EN ISO 14341-A : G 42 2 C1 4Si1
EN ISO 14341-A : G 46 3 M21 4Si1
EN ISO 636-A : W 46 3 W4Si1
Wire Electrode EN ISO 636-A : W4Si1
EN ISO 14341-A : G4Si1

Approvals

Grade 12430
Society VdTÜV
Approvals are based on factory location. Please contact ESAB for more information.

Consumable Characteristics

Alloy Type Carbon-manganese steel (Mn/Si-alloyed)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Mn P S Si
0.09 % 1.65 % - - 0.97 %
Typical Weld Metal Analysis %
80Ar/20CO2 (M21)
0.07 % 1.25 % 0.009 % 0.009 % 0.82 %
CO2 (C1)
0.06 % 1.05 % 0.009 % 0.009 % 0.72 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Pipeweld 70S-6
1P660924A0 FIND A DISTRIBUTOR
1P660915A0 FIND A DISTRIBUTOR
1P660919AW FIND A DISTRIBUTOR
1P661024A0 FIND A DISTRIBUTOR
1P661019A0 FIND A DISTRIBUTOR
1P661224A0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..