Pipeweld 70S-6 Plus

ESAB

Pipeweld 70S-6 Plus

The following items have been added to your list


x

Pipeweld 70S-6 Plus is a copper free solid wire of very high purity for downhill circumferential GMAW welding on pipe qualities API 5L, Grade X52 to Grade X70. The electrode permits welding with high current (spray-arc) and also with short circuiting transfer in all positions.

BUY NOW


Typical Charpy V-Notch Properties

Impact Value Testing Temperature
as welded aws co2 (c1)
100 J (74 ft-lb) -20 degC (-4 degF)
80 J (59 ft-lb) -29 degC (-20 degF)
as welded en 80ar/20co2 (m21)
100 J (74 ft-lb) -20 degC (-4 degF)
80 J (59 ft-lb) -30 degC (-22 degF)
140 J (104 ft-lb) 20 degC (68 degF)
as welded en co2 (c1)
80 J (59 ft-lb) -20 degC (-4 degF)
120 J (89 ft-lb) 20 degC (68 degF)

Typical Tensile Properties

Condition As Welded As Welded As Welded
Shielding Gas AWS CO2 (C1) EN 80Ar/20CO2 (M21) EN CO2 (C1)
Tensile Strength 575 MPa (83 ksi) 600 MPa (87 ksi) 575 MPa (83 ksi)
Yield Strength 470 MPa (68 ksi) 545 MPa 495 MPa
Elongation 29 % 26 % 25 %

Classifications

Wire Electrode SFA/AWS A5.18 : ER70S-6
Weld Metal EN ISO 14341-A : G 42 2 C1 4Si1
EN ISO 14341-A : G 46 3 M21 4Si1
Wire Electrode EN ISO 14341-A : G 4Si1

Consumable Characteristics

Alloy Type Carbon-manganese steel (Mn/Si-alloyed)

Typical Weld Metal Analysis %

Typical Wire Composition %
C Cu Mn P S Si
0.090 % - 1.7 % - - 1.0 %
Typical Weld Metal Analysis %
80Ar/20CO2 (M21)
0.07 % 0.02 % 1.25 % 0.009 % 0.009 % 0.82 %
CO2 (C1)
0.06 % 0.02 % 1.05 % 0.009 % 0.009 % 0.72 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : Pipeweld 70S-6 Plus
1P650915A0 FIND A DISTRIBUTOR
1P651024A0 FIND A DISTRIBUTOR
1P651219A0 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..