OK AristoRod 12.62 is a bare triple deoxidised ER70S-2 solid wire for the GMAW of non-alloyed steels, as used in general construction, pressure vessel fabrication and shipbuilding. It yields high-quality welds in semi-killed and rimmed steels, as well as with grades with various carbon contents. Added deoxidants, Al - Ti- Zr, make the wire also suitable for steels with a dirty or rusty surface, without sacrificing weld quality. OK AristoRod 12.62 is treated with ESAB’s unique Advanced Surface Characteristics (ASC) technology, taking MIG/MAG welding operations to new levels of performance and all-round efficiency, especially in robotic and mechanised welding. Characteristic features include excellent start properties; trouble-free feeding at high wire speeds and lengthy feed distances; a very stable arc at high welding currents; extremely low levels of spatter; low fume emission; reduced contact tip wear and improved protection against corrosion of the wire.

BUY NOW


Typical Charpy V-Notch Properties

As Welded
Impact Value 133 ft-lb
Impact Value 180 J
Shielding Gas 80% Ar - 20% CO2
Testing Temperature -40 °F
Testing Temperature -40 °C

Typical Tensile Properties

ConditionElongationShielding GasTensile Strength Yield Strength
As Welded26 %EN 80Ar/20CO2 (M21) 625 MPa (91 ksi)570 MPa (83 ksi)

Deposition Data

Current Deposition Rate Diameter Voltage Wire Feed Speed
120-380 A 1.3-8.0 kg/h (2.9-17.6 lb/h) 1.2 mm (.045 in.) 18-35 V 2.5-15.0 m/min (98-590.5 in./min)
70-250 A 0.8-3.3 kg/h (1.8-7.3 lb/h) 0.9 mm (.035 in.) 18-26 V 3.0-12.0 m/min (118-472 in./min)

Classifications

Weld Metal EN ISO 14341-A : G 42 3 C1 2Ti
EN ISO 14341-A : G 46 4 M21 2Ti
Wire Electrode EN ISO 14341-A : G 2Ti
SFA/AWS A5.18 : ER70S-2

Consumable Characteristics

Alloy Type Carbon-manganese steel (Mn/Si-alloyed)

Typical Weld Metal Analysis %

Typical Wire Composition %
Al C Cr Cu J (Watanabe) Mn Mo Ni P S Si V
0.12 % 0.06 % 0.12 % 0.05 % 0.13 % 1.1 % 0.01 % 0.03 % 0.008 % 0.009 % 0.60 % 0.01 %
x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : OK Aristorod 12.62
1A62096910 FIND A DISTRIBUTOR
1A62106910 FIND A DISTRIBUTOR
1A62109320 FIND A DISTRIBUTOR
1A62116910 FIND A DISTRIBUTOR
1A62126910 FIND A DISTRIBUTOR
1A62129320 FIND A DISTRIBUTOR

ESAB EQUIPMENT WARRANTIES ARE VALID ONLY WHEN PURCHASED THROUGH AN ESAB AUTHORIZED DEALERSHIP.

x
x

x

Loading..