Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as welded and stress relieved conditions. It contains high levels of Manganese and Silicon to provide good wetting and good rust and scale tolerance. Spoolarc 83 is also used for all-position welding of high tensile pipe and tubing commonly found in earthmoving and construction equipment. It is available in forms suitable for MIG and TIG welding.

BUY NOW


Industries

  • Industrial and General Fabrication
  • Mobile Equipment
  • Automotive
  • Ship/Barge Building

Welding Process

  • GTAW (TIG - Tungsten Inert Gas )
  • GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)
  • SAW - Submerged Arc Welding

Specifications


Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 110 ksi 95 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 23 % 92 ksi 77 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 44 ft-lb -20 °F
98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 87 ft-lb -20 °F

Typical Weld Metal Analysis %

wire composition
PMnCuMoCSSiNi
0.01 %1.69 %0.17 %0.4 %0.08 %0.011 %0.63 %0.09 %

Approvals: CWB; CAN/CSA-ISO14341,B-G 55A 3 G4M31 (ER80S-D2); CWB; CSA W48; MIL-E-23765/2; 80S-3
Classifications: AWS A5.28; ER80S-D2/ER90S-D2

Approvals are based on factory location. Please contact ESAB for more information.


x

Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 110 ksi 95 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 23 % 92 ksi 77 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 44 ft-lb -20 °F
98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 87 ft-lb -20 °F

Typical Weld Metal Analysis %

wire composition
PMnCuMoCSSiNi
0.01 %1.69 %0.17 %0.4 %0.08 %0.011 %0.63 %0.09 %

Approvals: CWB; CAN/CSA-ISO14341,B-G 55A 3 G4M31 (ER80S-D2); CWB; CSA W48; MIL-E-23765/2; 80S-3
Classifications: AWS A5.28; ER80S-D2/ER90S-D2

Approvals are based on factory location. Please contact ESAB for more information.


x

Part Numbers and Accessories

Select All | Select None

Check box to add

Part Numbers : SPOOLARC 83
83 3/32X65#CL 1264F30 FIND A DISTRIBUTOR
83 1/8X65#CL 1264F32 FIND A DISTRIBUTOR
83 1/16X44#SP 1262F08 FIND A DISTRIBUTOR
83 BARE 035X44#SP 1282F05 FIND A DISTRIBUTOR
83 045X900#OMP 2/PLT 126UF47 FIND A DISTRIBUTOR
83 1.2X15KG SP 1268L07 FIND A DISTRIBUTOR
83 045X44#SP 1262F07 FIND A DISTRIBUTOR
83 045X550#OMP 20 2/PLT 126UF67 FIND A DISTRIBUTOR
83 035X33#SP 1268F05 FIND A DISTRIBUTOR
83 035X44#SP 1262F05 FIND A DISTRIBUTOR
83 035X500#MP 1269F05 FIND A DISTRIBUTOR
83 045X33#SP 1268F07 FIND A DISTRIBUTOR
83 1/8X453KG TM 1266F92 FIND A DISTRIBUTOR
83 5/32X30KG BOB 1264F34 FIND A DISTRIBUTOR
83 5/32X453KG TM 1266F94 FIND A DISTRIBUTOR
83 052X20KG CF 1262F01 FIND A DISTRIBUTOR
83 035X408KG OMP 2/PLT 126UF45 FIND A DISTRIBUTOR
83 052X408KG OMP 2/PLT 126UF41 FIND A DISTRIBUTOR
83 035X5KG CPX20KG CJ 126TF45 FIND A DISTRIBUTOR
x
×

Find the Closest Distributor

x

x

Loading..