Stoody Super Build Up deposit is a low alloy steel that can be used both as a build-up and hardfacing material because it has good compressive strength and hardness.

BUY NOW


Features

  • It is not intended to be used as an underbase for subsequent hardfacing. It can be used on carbon and low alloy steels, but not on manganese steels or cast iron.

Specifications


Typical Tensile Properties

Hardness (HRC)
35-40 HRC

Typical Weld Metal Analysis

OtherCCrFe
2.5 %0.5 %2.0 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
35-40 HRC

Typical Weld Metal Analysis

OtherCCrFe
2.5 %0.5 %2.0 %BAL %