Stoody M7-G

Stoody M7-G deposit is a molybdenum high speed tool steel similar to AISI M7 grade.

Where To Buy


Features

This material is characterized by a high hardness (58 to 66 HRC) and excellent wear resistance.

  • Can be used at elevated temperatures up to 1000F, under conditions of moderate thermal shock.

  • Specifications


    Typical Tensile Properties

    75% Ar - 25% CO2
    Hardness (HRC)
    58-66 HRC

    Typical Weld Metal Analysis %

    OtherCCrFe
    14.5 %1.0 %4.0 %BAL %

    x

    Typical Tensile Properties

    75% Ar - 25% CO2
    Hardness (HRC)
    58-66 HRC

    Typical Weld Metal Analysis %

    OtherCCrFe
    14.5 %1.0 %4.0 %BAL %