Stoody

Stoody HB-Ti

Stoody HB-Ti

Stoody HB-Ti offers the best combination of properties for open hole or cased hole drilling. Deposits have a fine dispersion of titanium carbides in a martensitic matrix delivering superior erosive and metal-to-metal wear resistance. HB-Ti is designed for open are welding and requires no gas shielding making it suitable for field repairs where the use of gas may not be possible or practical.

Where To Buy


Features

  • Developed for open hole and cased hole hard banding applications
  • Requires no shielding gas making it suitable for field repairs where access to gas is not possible or practical.
  • Offers the best combination of erosive and metal-to-metal wear resistance


Specifications


Typical Tensile Properties

Hardness (HRC)
57-61 HRC

Typical Weld Metal Analysis %

OtherCTiCrFe
3.0 %2.0 %5.0 %8.0 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
57-61 HRC

Typical Weld Metal Analysis %

OtherCTiCrFe
3.0 %2.0 %5.0 %8.0 %BAL %

x