Stoody CP-2000 is designed to produce a high concentration of uniformly distributed small primary chromium carbides in an austenitic matrix. The formulation is optimized for superior weldability in single and multiple layer applications. CP-2000 exhibits improved wear resistance and toughness over conventional chromium carbide alloys.

BUY NOW


Features

  • Superior weldability in single and multiple layer applications.
  • Alloy exhibits improved wear resistance and toughness over conventional chromium carbine alloys.
  • Can be utilized in hot wear applications up to 900°F (482°C)


Specifications


Typical Tensile Properties

Hardness (HRC)
58-64 HRC

Typical Weld Metal Analysis

OtherMnMoCSiCrFe
4.0 %1.5 %1.0 %4.8 %1.0 %24.0 %BAL %

x

Typical Tensile Properties

Hardness (HRC)
58-64 HRC

Typical Weld Metal Analysis

OtherMnMoCSiCrFe
4.0 %1.5 %1.0 %4.8 %1.0 %24.0 %BAL %