Stoody C-M is a nickel-based fabricated alloy cored wire for automatic/semi-automatic welding that produces a deposit resistant to high heat and corrosion accompanied by abrasion and/or impact. It is machinable but work hardens and can be applied in multiple layers.

Where To Buy


Features

Welding Procedures/Characteristics:

  • An automatic/semi-automatic wire (DECP) that can be applied in multiple layers.
    • Applications:
      • Hot Forge Dies
      • Hot Shear Blades
      • Forging Hammer Dies
      • Mill Guides
      • Shafts


Specifications


Typical Tensile Properties

100% Ar
Hardness (HRC)
30-40 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCrFe
0.1 %16.0 %0.02 %0.2 %4.0 %BAL %15.8 %5.0 %

x

Typical Tensile Properties

100% Ar
Hardness (HRC)
30-40 HRC

Typical Weld Metal Analysis %

MnMoCSiWNiCrFe
0.1 %16.0 %0.02 %0.2 %4.0 %BAL %15.8 %5.0 %