Stoody Build-Up is a low alloy wire with deposits exhibiting excellent compressive strength and resistance to plastic deformation. Build-up is a perfect choice for use as a buffer or build up layer to be covered by subsequent overlay hardfacing. Work hardens under impact.

Where To Buy


Features

  • Excellent compressive strength and resistance to plastic deformation
  • Perfect choice for buffering and build-up layers
  • Good machinability in the "as welded" condition
  • Will work harden under impact


Specifications


Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
29 HRC

Typical Weld Metal Analysis %

OtherCCrFe
3.0 %0.2 %1.0 %BAL %

x

Typical Tensile Properties

98% Ar - 2% O2
Hardness (HRC)
29 HRC

Typical Weld Metal Analysis %

OtherCCrFe
3.0 %0.2 %1.0 %BAL %